Serial Number: AJ24407
Run/Test Number: P6570
Technique: Thrown, incised, dip-glazed
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2926B
Clay Body - Polar Ice
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 94 mm (3.7 in)
Depth at rim (including handle) - 128 mm (5.0 in)
Height - 126 mm (5.0 in)
Weight - 437 grams (15.4 oz)