Serial Number: AJ24097
Run/Test Number: P6746
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2934Y Yellow
Clay Body - Polar Ice
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 95 mm (3.7 in)
Depth at rim (including handle) - 125 mm (4.9 in)
Height - 124 mm (4.9 in)
Weight - 395 grams (13.9 oz)
Price:$40.00 (Not for sale, pieces being held for demo purposes)