Bamboo tan incised stoneware mug

Serial Number: AJ24354
Run/Test Number: L4377C
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside
Description: H550 compatible clay body made from Blue Hills, Saskatchewan ball clay and Plainsman 3D.

Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - GR10-C
Glaze Outside - G2571B bamboo matte
Engobe - L3954N
Clay Body - H550
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 94 mm (3.7 in)
Depth at rim (including handle) - 127 mm (5.0 in)
Height - 97 mm (3.8 in)
Weight - 348 grams (12.3 oz)

Price:$30.00 (Not for sale, pieces being held for demo purposes)