Serial Number: AJ24086
Run/Test Number: P6803
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2934Y Red
Clay Body - Polar Ice
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 89 mm (3.5 in)
Depth at rim (including handle) - 121 mm (4.8 in)
Height - 104 mm (4.1 in)
Weight - 312 grams (11.0 oz)