Serial Number: AJ24315
Run/Test Number: P6932
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G3914A
Glaze Outside - G2926BL
Clay Body - M370
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 100 mm (3.9 in)
Depth at rim (including handle) - 130 mm (5.1 in)
Height - 118 mm (4.6 in)
Weight - 343 grams (12.1 oz)
Price:$40.00 (Not for sale, pieces being held for demo purposes)