Rutile blue buff MNS stoneware mug

Serial Number: AJ24013
Run/Test Number: L4208C
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - GA6-B
Glaze Outside - GA6-C
Clay Body - L4208C MNS
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 96 mm (3.8 in)
Depth at rim (including handle) - 101 mm (4.0 in)
Height - 127 mm (5.0 in)
Weight - 359 grams (12.7 oz)