Floating-blue stoneware mug

Serial Number: AJ24391
Run/Test Number: P7001
Technique: Thrown, liner-glazed inside, dip-glazed outside

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - GA6-B
Glaze Outside - GR6-M
Clay Body - Coffee
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 95 mm (3.7 in)
Depth at rim (including handle) - 129 mm (5.1 in)
Height - 94 mm (3.7 in)
Weight - 315 grams (11.1 oz)