Blue Porcelain Mug

Serial Number: AJ24100
Run/Test Number: P6746
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2934Y Blue
Clay Body - M370
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 92 mm (3.6 in)
Depth at rim (including handle) - 120 mm (4.7 in)
Height - 105 mm (4.1 in)
Weight - 382 grams (13.5 oz)