Serial Number: AJ24375
Run/Test Number: L4486B
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table.
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G3914A
Glaze Outside - GR6-M
Clay Body - L4486B MNP
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 96 mm (3.8 in)
Depth at rim (including handle) - 131 mm (5.2 in)
Height - 111 mm (4.4 in)
Weight - 339 grams (11.9 oz)
Price:$40.00 (Not for sale, pieces being held for demo purposes)