Serial Number: AJ24308
Run/Test Number: L4115J3S
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2934Y Black
Clay Body - M340S Test
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 101 mm (4.0 in)
Depth at rim (including handle) - 134 mm (5.3 in)
Height - 110 mm (4.3 in)
Weight - 354 grams (12.5 oz)