Serial Number: AJ50047
Run/Test Number: L4686A
Description: Fired at cone 6 oxidation on buff stoneware. By Tony Hansen.
Temperature - Cone 10R
Glaze Inside - G1947U
Glaze Outside - G2571D
Clay Body - H550
Foot Style - Flat unglazed
Width at rim (perpendicular to handle) - 0 mm (0.0 in)
Depth at rim (including handle) - 0 mm (0.0 in)
Height - 0 mm (0.0 in)
Not for sale