Iron red glazed stoneware mug

Serial Number: AJ24438
Run/Test Number: L4471J2
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G3914A
Glaze Outside - G3948A
Clay Body - M340
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 96 mm (3.8 in)
Depth at rim (including handle) - 130 mm (5.1 in)
Height - 120 mm (4.7 in)
Weight - 391 grams (13.8 oz)