Variegated glossy blue mug

Serial Number: AJ24106
Run/Test Number: P6729
Technique: Thrown, incised, dip-glazed

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - GR6-M
Glaze Outside - GR6-M
Clay Body - M390
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 97 mm (3.8 in)
Depth at rim (including handle) - 132 mm (5.2 in)
Height - 121 mm (4.8 in)
Weight - 409 grams (14.4 oz)