Copper blue-green Crysanthos porcelain mug

Serial Number: AJ240210
Run/Test Number: L3611A
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G3806E
Clay Body - L3611A
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 87 mm (3.4 in)
Depth at rim (including handle) - 119 mm (4.7 in)
Height - 99 mm (3.9 in)
Weight - 329 grams (11.6 oz)

Price:$50.00 (Not for sale, pieces being held for demo purposes)


PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy