Serial Number: AJ24075
Run/Test Number: P6850
Technique: Hand-rolled, embossed and assembled, liner-glazed inside, dip-glazed outside
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - L3500G+2Fe
Glaze Outside - GA6-C+2% iron oxide
Clay Body - M390
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 97 mm (3.8 in)
Depth at rim (including handle) - 134 mm (5.3 in)
Height - 101 mm (4.0 in)
Weight - 353 grams (12.4 oz)
Price:$35.00 (Not for sale, pieces being held for demo purposes)