Serial Number: AJ24089
Run/Test Number: P6731
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - GR10-C
Glaze Outside - GR10-C
Engobe - L3954N
Clay Body - H550
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 100 mm (3.9 in)
Depth at rim (including handle) - 133 mm (5.2 in)
Height - 110 mm (4.3 in)
Weight - 363 grams (12.8 oz)
Price:$40.00 (Not for sale, pieces being held for demo purposes)