Serial Number: AJ24018
Run/Test Number: L3778D
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G3806E
Clay Body - L3778D
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 89 mm (3.5 in)
Depth at rim (including handle) - 117 mm (4.6 in)
Height - 101 mm (4.0 in)
Weight - 194 grams (6.8 oz)
Price:$50.00 (Not for sale, pieces being held for demo purposes)