White glazed speckled stoneware mug

Serial Number: AJ24440
Run/Test Number: L4471J2
Technique: Thrown, incised, dip-glazed

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G3926B
Glaze Outside - G3926B
Clay Body - M340S
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 100 mm (3.9 in)
Depth at rim (including handle) - 130 mm (5.1 in)
Height - 110 mm (4.3 in)
Weight - 337 grams (11.9 oz)

Price:$40.00 (Not for sale, pieces being held for demo purposes)


PayPal