Digitalfire will shut down on June 26. I no longer have the authority to grant exemption to a section in the Terms and Conditions of using material in the Insight-Live account from which I built the source material. While there are ways to comply with the take-down order, they are beyond my means because of how complex and large the site has become in the past 35+ years. It has been a wild ride for a shy prairie boy, thanks to everyone for your support. Insight-live.com is not affected by this.
![]() | ![]() |
Serial Number: AJ50039
Run/Test Number: L3905G1
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table.
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - GA6-C
Clay Body - M340
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 0 mm (0.0 in)
Depth at rim (including handle) - 0 mm (0.0 in)
Height - 0 mm (0.0 in)
Not for sale