Serial Number: AJ24052
Run/Test Number: P6679
Technique: Hand-rolled and assembled, engobed inside and top outside, incised, dip-glazed
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G2571A Bamboo
Glaze Outside - G2571A Bamboo
Engobe - L3954N
Clay Body - H550
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 99 mm (3.9 in)
Depth at rim (including handle) - 130 mm (5.1 in)
Height - 101 mm (4.0 in)
Weight - 339 grams (11.9 oz)