Serial Number: AJ24426
Run/Test Number: P6947
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G3914A
Glaze Outside - GR6-M
Clay Body - M340
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 100 mm (3.9 in)
Depth at rim (including handle) - 135 mm (5.3 in)
Height - 116 mm (4.6 in)
Weight - 392 grams (13.8 oz)
Price:$35.00 (Not for sale, pieces being held for demo purposes)