Baby blue Polar Ice porcelain mug

Serial Number: AJ24367
Run/Test Number: P6967
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2934Y blue
Clay Body - Polar Ice
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 93 mm (3.7 in)
Depth at rim (including handle) - 126 mm (5.0 in)
Height - 118 mm (4.6 in)
Weight - 389 grams (13.7 oz)