Serial Number: AJ24114
Run/Test Number: P6928
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2934Y Black
Clay Body - P300
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 102 mm (4.0 in)
Depth at rim (including handle) - 130 mm (5.1 in)
Height - 113 mm (4.4 in)
Weight - 325 grams (11.5 oz)
Price:$40.00 (Not for sale, pieces being held for demo purposes)