Pink Crystal Matte H555 mug

Serial Number: AJ24035
Run/Test Number: P6842
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G1947U
Glaze Outside - G2571D
Clay Body - H555
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 116 mm (4.6 in)
Depth at rim (including handle) - 131 mm (5.2 in)
Height - 114 mm (4.5 in)
Weight - 375 grams (13.2 oz)