Serial Number: AJ24038
Run/Test Number: P6816
Technique: Thrown, engobed, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - GR10-C
Glaze Outside - GR10-C
Engobe - L3954N
Clay Body - H550
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 101 mm (4.0 in)
Depth at rim (including handle) - 131 mm (5.2 in)
Height - 112 mm (4.4 in)
Weight - 418 grams (14.7 oz)