White glossy glazed reduction fired mug

Serial Number: AJ24422
Run/Test Number: L4453E
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G1947U
Glaze Outside - GR10-CW
Clay Body - H550
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 95 mm (3.7 in)
Depth at rim (including handle) - 132 mm (5.2 in)
Height - 108 mm (4.3 in)
Weight - 350 grams (12.3 oz)