Bamboo Silky Matte H555 mug

Serial Number: AJ24041
Run/Test Number: P6842
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G1947U
Glaze Outside - G2571B
Engobe - L3954N
Clay Body - H555
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 91 mm (3.6 in)
Depth at rim (including handle) - 120 mm (4.7 in)
Height - 112 mm (4.4 in)
Weight - 328 grams (11.6 oz)

Price:$35.00 (Not for sale, pieces being held for demo purposes)