Floating-blue stoneware mug

Serial Number: AJ24432
Run/Test Number: P7024
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G3914A
Glaze Outside - GR6-M
Clay Body - M340
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 99 mm (3.9 in)
Depth at rim (including handle) - 132 mm (5.2 in)
Height - 113 mm (4.4 in)
Weight - 404 grams (14.2 oz)