Serial Number: AJ24043
Run/Test Number: P6746
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2926B Purple
Clay Body - Polar Ice
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 91 mm (3.6 in)
Depth at rim (including handle) - 120 mm (4.7 in)
Height - 124 mm (4.9 in)
Weight - 375 grams (13.2 oz)
Price:$40.00 (Not for sale, pieces being held for demo purposes)