Serial Number: AJ24386
Run/Test Number: P7004
Technique: Thrown, transfers applied at leather hard, liner-glazed inside, dip-glazed outside
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2934 Red
Glaze Outside - G2934
Clay Body - M370
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 95 mm (3.7 in)
Depth at rim (including handle) - 128 mm (5.0 in)
Height - 110 mm (4.3 in)
Weight - 341 grams (12.0 oz)
Price:$35.00 (Not for sale, pieces being held for demo purposes)