Serial Number: AJ24359
Run/Test Number: P6747
Technique: Thrown, incised, dip-glazed
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G1947U
Glaze Outside - G1947U
Clay Body - P700
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 94 mm (3.7 in)
Depth at rim (including handle) - 129 mm (5.1 in)
Height - 122 mm (4.8 in)
Weight - 345 grams (12.2 oz)