Serial Number: AJ24046
Run/Test Number: L4115J1
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - GA6-B
Clay Body - 3D+Ball Clay, bentonite, Nepheline
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 100 mm (3.9 in)
Depth at rim (including handle) - 133 mm (5.2 in)
Height - 106 mm (4.2 in)
Weight - 332 grams (11.7 oz)
Price:$40.00 (Not for sale, pieces being held for demo purposes)