Serial Number: AJ24014
Run/Test Number: 6850
Technique: Hand-rolled, embossed and assembled, liner-glazed inside, dip-glazed outside
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - GA6-B
Glaze Outside - G2934Y Black
Clay Body - M390
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 97 mm (3.8 in)
Depth at rim (including handle) - 133 mm (5.2 in)
Height - 101 mm (4.0 in)
Weight - 338 grams (11.9 oz)
Price:$40.00 (Not for sale, pieces being held for demo purposes)
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
Buy me a coffee and we can talk