Rutile blue stoneware mug

Serial Number: AJ50038
Run/Test Number: L3905H
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table.

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - GA6-C
Clay Body - M340
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 0 mm (0.0 in)
Depth at rim (including handle) - 0 mm (0.0 in)
Height - 0 mm (0.0 in)

Not for sale


PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy