Serial Number: AJ24129
Run/Test Number: P6842
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G1947U
Glaze Outside - G2571B Bamboo
Clay Body - H555
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 101 mm (4.0 in)
Depth at rim (including handle) - 127 mm (5.0 in)
Height - 124 mm (4.9 in)
Weight - 407 grams (14.3 oz)