Serial Number: AJ24404
Run/Test Number: L3924J
Technique: Thrown, leather-hard under-glaze decorated, incised, 1650F bisque fired, dip-glazed
Firing Schedule - C04PLTP
Temperature - Cone 04
Glaze Inside - G3879C
Glaze Outside - G3879C
Clay Body - L3924J
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 97 mm (3.8 in)
Depth at rim (including handle) - 129 mm (5.1 in)
Height - 135 mm (5.3 in)
Weight - 400 grams (14.1 oz)
Price:$50.00 (Not for sale, pieces being held for demo purposes)