Serial Number: AJ24024
Run/Test Number: P6847
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G1947U
Glaze Outside - G2571D
Clay Body - H570
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 100 mm (3.9 in)
Depth at rim (including handle) - 127 mm (5.0 in)
Height - 130 mm (5.1 in)
Weight - 373 grams (13.1 oz)
Price:$35.00 (Not for sale, pieces being held for demo purposes)
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
Buy me a coffee and we can talk