Serial Number: AJ24067
Run/Test Number: L4283
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G3806C
Clay Body - L4283
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 81 mm (3.2 in)
Depth at rim (including handle) - 111 mm (4.4 in)
Height - 85 mm (3.3 in)
Weight - 231 grams (8.1 oz)