Ravenscrag Raspberry mug

Serial Number: AJ50030
Run/Test Number: M340
Description: Fired at cone 6 oxidation on buff stoneware. By Tony Hansen.

Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - L4398
Clay Body - M340
Foot Style - Flat unglazed
Width at rim (perpendicular to handle) - 0 mm (0.0 in)
Depth at rim (including handle) - 0 mm (0.0 in)
Height - 0 mm (0.0 in)