Rutile blue buff stoneware mug

Serial Number: AJ24054
Run/Test Number: P6770
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - GA6-C
Glaze Outside - GA6-C
Engobe - L3954B
Clay Body - M340
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 100 mm (3.9 in)
Depth at rim (including handle) - 130 mm (5.1 in)
Height - 119 mm (4.7 in)
Weight - 478 grams (16.8 oz)

Price:$35.00 (Not for sale, pieces being held for demo purposes)


PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved