Bamboo tan incised stoneware mug

Serial Number: AJ24410
Run/Test Number: L4040A
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - GR10-C
Glaze Outside - G2571A Bamboo
Engobe - L3954N
Clay Body - H555
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 100 mm (3.9 in)
Depth at rim (including handle) - 134 mm (5.3 in)
Height - 111 mm (4.4 in)
Weight - 362 grams (12.8 oz)

Price:$45.00 (Not for sale, pieces being held for demo purposes)


PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy