Serial Number: AJ24439
Run/Test Number: L4471J2
Technique: Thrown, incised, dip-glazed
Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G3926B
Glaze Outside - G3926B
Clay Body - M340S
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 95 mm (3.7 in)
Depth at rim (including handle) - 131 mm (5.2 in)
Height - 122 mm (4.8 in)
Weight - 369 grams (13.0 oz)
Price:$40.00 (Not for sale, pieces being held for demo purposes)