Rutile blue red-brown M332 stoneware mug

Serial Number: AJ24011
Run/Test Number: P6851
Technique: Hand-rolled, embossed and assembled, liner-glazed inside, dip-glazed outside

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - GA6-B
Glaze Outside - GA6-C
Clay Body - M332
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 99 mm (3.9 in)
Depth at rim (including handle) - 135 mm (5.3 in)
Height - 102 mm (4.0 in)
Weight - 350 grams (12.3 oz)

Price:$40.00 (Not for sale, pieces being held for demo purposes)


PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved