L3905C

Serial Number: AJ24402
Run/Test Number: L3905C
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G3914A
Clay Body - M370
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 87 mm (3.4 in)
Depth at rim (including handle) - 124 mm (4.9 in)
Height - 113 mm (4.4 in)
Weight - 297 grams (10.5 oz)

Price:$30.00 (Not for sale, pieces being held for demo purposes)