Copper blue-green Polar Ice porcelain mug

Serial Number: AJ24144
Run/Test Number: P6746
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G3806C
Clay Body - Polar Ice
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 88 mm (3.5 in)
Depth at rim (including handle) - 120 mm (4.7 in)
Height - 99 mm (3.9 in)
Weight - 312 grams (11.0 oz)