Serial Number: AJ24157
Run/Test Number: P6823
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - L3500G+2Fe
Glaze Outside - GA6-C
Clay Body - M350
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 95 mm (3.7 in)
Depth at rim (including handle) - 125 mm (4.9 in)
Height - 119 mm (4.7 in)
Weight - 367 grams (12.9 oz)
Price:$35.00 (Not for sale, pieces being held for demo purposes)