Serial Number: AJ24352
Run/Test Number: L4486A
Technique: Thrown, incised, pour-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table.
Firing Schedule - C5DHSC
Temperature - Cone 5
Glaze Inside - L3500G
Glaze Outside - G2934Y gunmetal
Clay Body - L4486A MNP
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 94 mm (3.7 in)
Depth at rim (including handle) - 132 mm (5.2 in)
Height - 111 mm (4.4 in)
Weight - 354 grams (12.5 oz)
Price:$45.00 (Not for sale, pieces being held for demo purposes)