Black silky matte mug

Serial Number: AJ24419
Run/Test Number: P7027
Technique: Thrown, liner-glazed inside, dip-glazed outside

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G3914A
Glaze Outside - G2934Y Black
Engobe - L3954B
Clay Body - M370
Foot Style - Unglazed flat black engobed
Width at rim (perpendicular to handle) - 97 mm (3.8 in)
Depth at rim (including handle) - 128 mm (5.0 in)
Height - 103 mm (4.1 in)
Weight - 334 grams (11.8 oz)