Serial Number: AJ24441
Run/Test Number: P7027
Technique: Thrown, liner-glazed inside, dip-glazed outside
Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G2926BL
Glaze Outside - G2926BL
Engobe - L3954B
Clay Body - M370
Foot Style - Unglazed flat black engobed
Width at rim (perpendicular to handle) - 93 mm (3.7 in)
Depth at rim (including handle) - 127 mm (5.0 in)
Height - 108 mm (4.3 in)
Weight - 346 grams (12.2 oz)
Not for sale