Translucent porcelain reduction-fired mug

Serial Number: AJ24323
Run/Test Number: P6747
Technique: Thrown, incised, dip-glazed

Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G1947U
Glaze Outside - G1947U
Clay Body - P700
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 91 mm (3.6 in)
Depth at rim (including handle) - 121 mm (4.8 in)
Height - 110 mm (4.3 in)
Weight - 326 grams (11.5 oz)

Not for sale